Does the PET material on the surface of the membrane switch tend to age and turn yellow?
The PET material on the surface of the membrane switch does have the problem of aging and yellowing, which is determined by the molecular structure characteristics of the PET material itself. Here is a detailed analysis and corresponding solution:
The fundamental reason for PET to turn yellow
The molecular structure of PET contains aromatic rings and ester groups. Under the following conditions, it will undergo degradation:
Ultraviolet radiation: Ultraviolet light will break the molecular chains, forming new conjugated double bond systems and carbonyl structures. These structures can absorb visible light, causing the material to turn yellow.
Heat oxidation: In high-temperature environments, the PET molecular chains undergo oxidation reactions, generating chromogenic groups such as carboxyl groups.
Hydrolysis: When PET contains water, the ester bonds will undergo hydrolysis and break, resulting in a darker color and reduced toughness.
Humidity synergy: The combined effect of ultraviolet rays, moisture, and oxygen will significantly accelerate yellowing.
The relationship between yellowing degree and usage environment
Based on the data from natural aging experiments:
| Usage environment | Yellowing speed | Typical manifestation |
| Indoor, dark place | Slow | Minor yellowing can be observed after several years |
| Indoor, near window (diffused light) | Medium | Obvious yellowing can be seen within 1-2 years |
| Outdoor, direct sunlight | Fast | Yellowing becomes obvious within a few months, transparency significantly decreases |
| High temperature and high humidity environment | Extremely fast | Yellowing + fogging + mechanical properties decline |
After outdoor natural aging, the yellowness index (YI) and color difference (ΔC) of PET significantly increase, the light transmittance decreases significantly, and micro-cracks will appear on the surface.
PET vs PC Weather Resistance Comparison
| Comparison Items | PET | PC (Polycarbonate) |
| Yellowing tendency | Higher, significantly yellowing under long-term sunlight | Lower, yellowing index is better than that of ordinary PET |
| Temperature range | -60℃~150℃ | -40℃~125℃ |
| Impact resistance | Good | Excellent (3-5 times that of PET) |
| Cost | Lower | About 30% higher than PET |
| Application scenarios | Indoor normal temperature equipment | Outdoor/automobile/high-temperature environment |
For outdoor or direct sunlight scenarios, a PC is a more reliable choice.
Practical measures to prevent PET from yellowing
Material level
Select UV-resistant PET: PET films with added UV absorbers (such as benzotriazole types) and antioxidants can significantly delay yellowing
Surface hardening coating: A 3-5 μm hard coating can increase the anti-abrasion ability by 3-4 times, while providing certain UV shielding
Backside printing shading layer: Printing black or dark shading ink on the back of PET can block ultraviolet rays from penetrating
Structural design aspect
Install UV filtering panel: Add a layer of UV-blocking film or UV filter on the PET surface
Avoid direct sunlight exposure: Design the equipment shell to block sunlight, such as adding shading eaves
Seal and prevent moisture: Seal the edges with silicone to prevent moisture from penetrating and accelerating hydrolysis
Maintenance level
Regularly clean the surface to prevent oil stains from accelerating photo-oxidation
Place desiccant in a humid environment
Avoid using cleaning agents containing strong oxidants
What to do if it has turned yellow?
Slight yellowing: You can use a special plastic refurbishing agent (containing polishing and anti-oxidation components) for wiping, which can have a certain recovery effect.
Moderate yellowing: It is irreversible and can only be replaced by a new panel layer.
Severe yellowing + brittleness: The entire Membrane Switch must be replaced because the material's mechanical properties have severely declined.
💡Summary: PET material is prone to aging and yellowing in membrane switches, especially when exposed to ultraviolet rays, high temperatures, and high humidity. In an indoor dark environment, it can be used for several years without significant yellowing, but in direct sunlight outdoors, it will become noticeably yellow within a few months. Preventive measures include using UV-resistant PET, applying hard coatings, printing a shading layer on the back, and avoiding direct sunlight; for outdoor or high-temperature scenarios, it is recommended to directly use PC material, as its weather resistance and anti-yellowing ability are significantly better than those of PET.