How is the standard grade determination for the oil-resistant test of the membrane keypads conducted?
The determination of the oil resistance test standard level for membrane keypads mainly relies on standardized testing methods. It is quantitatively evaluated by observing the wetting, penetration or morphological changes of specific reagents on the surface of the thin film. Currently, the mainstream determination standards and methods in the industry include the following three types:

I. Oil Resistance Grade Test (Drop Oil Method)
This is the most commonly used method for evaluating the ability of film materials to resist liquid oil contamination. It is based on national standard GB/T 19977, international standard ISO 14419, and American standard AATCC 118.
Judgment principle: A series of standard hydrocarbons with decreasing surface tension (such as mineral oil, n-heptane, etc., usually divided into 0-8 grades or higher) are used as the test liquid.
Operation procedure: Place the film sample flatly, start with the test oil of the lowest number (with the highest surface tension), use a dropper to take a small amount of oil droplet (about 5 microliters) and gently drop it on the sample surface. Observe for 30 seconds at a specific angle. If the oil droplet remains spherical, not wetting nor penetrating, then use a higher-grade (with lower surface tension) test oil to continue the test.
Grade determination: The highest standard oil number that does not cause the film surface to be wetted or penetrated is taken as the final result. The higher the grade number, the better the oil resistance performance of the film.
II. KIT Oil Resistance Test
This method is based on the ISO 16532-2 standard and is commonly used to evaluate the oil and stain resistance of films and coatings.
Judgment principle: A mixed solution composed of flaxseed oil (or castor oil), toluene, and n-heptane (with a maximum of 12 grades) is used. As the solvent proportion increases, the surface tension of the mixed solution decreases, and the penetration ability of the solution to the material becomes stronger.
Operation procedure: Add the test solution to the film surface, let it stand for 15 seconds, and then observe.
Grade determination: The highest numbered solution that does not cause the film sample surface to darken (i.e., no penetration or wetting failure occurs) after 15 seconds is used for assessment. This highest numbered solution is the "KIT rating" (up to 12 grades), and the larger the number, the better the oil resistance performance.
III. Test Method for Paint Film Oil Resistance
If the surface of the membrane keypad has undergone special coating or film covering treatment, the oil resistance test can also be conducted according to the HG/T 3343 standard of the chemical industry.
Judgment principle: Simulate the soaking or contact state of the film in specific oils (such as transformer oil, lubricating oil or gasoline).
Operation procedure: Immerse the film or painted test plate in the specified temperature oil, or pour the oil onto the surface and cover it with a cloth and a weight, keeping it for the specified time before removing and wiping clean.
Grade determination: Check if there are any phenomena such as bubbling, wrinkling, peeling, softening, discoloration or loss of gloss on the film surface. Determine the oil resistance as qualified if a certain number of test plates maintain a smooth and flat surface without any abnormal changes.
Summary: For membrane keypads, the most crucial criterion for determining the oil resistance grade is the oil repellency test (AATCC 118 / ISO 14419) and the KIT test (ISO 16532-2). Both of these tests achieve the quantification of the grade by identifying the "highest level of test solution where the film surface does not become wet or darkened". The higher the grade value, the stronger the oil resistance and stain resistance of the membrane keypads.