    How is the temperature resistance performance of the membrane button panel tested?

    2026-05-13

    The temperature resistance performance of the membrane button panel directly affects whether it will deform, change color or fail in high-temperature environments (such as car dashboards, kitchen appliances).

    According to industry standards, the tests are typically divided into "material-level tests" (for the base material) and "finished product-level tests" (for the assembled panels). To help you understand this process more clearly, I have compiled the following test methods based on relevant testing standards (such as ASTM, ISO, GB/T):

    1.jpg
    1. Core test items

    The temperature resistance test of the membrane button panel  mainly focuses on the following key indicators:

    • Heat distortion temperature (HDT): This tests the critical temperature at which the film deforms under a certain load (simulating the installation state). This is a key indicator for determining whether the film panel can remain flat at high temperatures.
    • Vickers softening point (VST): Measures the temperature at which a needle penetrates the film to a depth of 1mm, reflecting the temperature point at which the material begins to soften.
    • High and low temperature cycling/shock: Simulates the temperature difference between day and night or extreme environments, testing whether the panel will experience delamination, blistering or cracking under repeated cold and hot alternations.
    • Heat aging/corrosion resistance: Exposes the panel to high temperatures for a long time, testing its color stability (whether it turns yellow) and mechanical properties (whether it becomes brittle).

    2. Specific Testing Methods and Procedures

    A. Thermal Deformation and Softening Test (Material Level)

    This is typically conducted using a specialized Vickers softening point tester for thermal deformation.

    Standards: Refer to ISO 75, ASTM D648, or GB/T 1634.

    Procedure:

    Place the film sample (usually cut into a long strip) on the test frame and apply a standard load (such as 1.82 MPa or 0.45 MPa).

    Submerge the sample in a heat-conductive medium (such as silicone oil) or place it in a heating box.

    Increase the temperature at a constant rate (such as 50°C/h or 120°C/h).

    Record the temperature at which the deformation of the sample reaches the specified value (such as 0.25 mm or 1.0 mm).

    B. High and Low Temperature Cycling Test (Finished Product Level)

    This is a test that simulates the actual service life of the membrane button panel. It is usually conducted using a programmable high and low temperature test chamber.

    Standard: Refer to JEDEC JESD22-A104 or GB/T 2423.

    Procedure:

    Place the finished panel in the test chamber.

    Set the cycling program: For example, from -40°C (keep at this temperature for 2 hours) rapidly increase to 85°C or 90°C (keep at this temperature for 2 hours).

    Repeat the cycle 50 times, 100 times or even more.

    Judgment: After removal, observe for any cracks, delamination, or detachment, and test if the buttons can still conduct normally.

    2.jpg

    C. High Temperature Tensile Test (Mechanical Properties)

    For flexible panels that need to withstand tension, test their strength at high temperatures.

    • Equipment: High and Low Temperature Tensile Testing Machine.
    • Procedure: Stretch the film in a high-temperature environment (e.g., 175°C), record its breaking strength and elongation rate, and evaluate whether the material is prone to breaking at high temperatures.

    3. Reference for the Temperature Resistance of Common Film Materials

    Different substrates determine the upper limit of the temperature resistance of the panel. The following is a comparison of the temperature resistance performance of common materials:

    Material type Typical temperature resistance range Characteristics and applications
    PET (Polyester) -60°C ~ +120°C Moderate temperature resistance, low cost, suitable for general household appliances and instrument panels.
    PC (Polycarbonate)     -60°C ~ +135°C Excellent temperature resistance, strong impact resistance, commonly used in car interiors and outdoor equipment.
    PI (Polyimide) -200°C ~ +250°C Extremely strong temperature resistance, usually used in high-end FPC or special industrial environments, high cost.
    PVC (Polyvinyl Chloride) -20°C ~ +60°C Poor temperature resistance, prone to shrinkage and deformation at high temperatures, only suitable for normal indoor environments

    4. Criteria for determining failure

    After the test is completed, if any of the following situations occur, the product is generally judged to have failed in terms of temperature resistance:

    • Appearance: The surface is noticeably yellowed, blistered, the edges are curled or the shrinkage rate exceeds 5%.
    • Structure: The panel and the underlying circuit separate (de-gumming), or there are visible cracks.
    • Function: The button feels collapsed or the circuit breaks after high-temperature exposure.

    If you are customizing a membrane button panel, it is recommended to clearly inform the manufacturer of the maximum operating temperature of the product (for example, automotive gauges may need to withstand exposure to temperatures above 85°C). This will allow the manufacturer to select the appropriate substrate (such as recommending the use of PC instead of PET) and conduct corresponding temperature resistance tests.