Welcome to LuphiTouch®!
Today is 2026.11.09 , Monday
Leave Your Message
News Categories
    Featured News

    How to effectively prevent the problem of silver paste migration in membrane switches?

    2026-06-16

    The silver migration of the membrane switch refers to the phenomenon where, under the influence of high temperature, high humidity and continuous direct current voltage, silver ions are ionized under the electric field drive and move from the anode to the cathode, eventually forming dendritic crystals that cause short circuits. To effectively prevent this issue, comprehensive control needs to be carried out from four dimensions: material formulation, physical protection, structural design and production process.

    productive process (14).jpg

    I. Optimization of silver paste formulation and material selection
    Addionics capture agent: Add specific ion capture agents (such as the IXE series) to the conductive silver paste. Through chemical bonding, precisely lock the free silver ions, preventing them from leaving the original circuit. This method can function even in low humidity conditions and does not affect the conductivity.
    Enhance paste density: Adjust the silver paste formulation, for example, by adding components such as lead nitrate and vanadium pentoxide glass powder. This can promote liquid-phase sintering during the sintering process, reduce micro-pores, and make the medium a highly dense irreversible water-absorbing composite crystal, thereby inhibiting the diffusion of silver ions.
    Select dense powder: Prioritize the use of spherical or flake-shaped mixed silver powders with high density and uniform particle size distribution. Avoid using blocky or poorly dense silver pastes to prevent silver ions from leaking out through gaps.

    II. Strengthening Physical Protection and Insulation Coatings
    Increase carbon layer coverage: Adopt a combined design process of "printing silver first and then carbon", using inert carbon ink to cover the silver traces. The carbon layer not only prevents oxidation and wear but also effectively blocks moisture and cuts off the water vapor conditions for silver migration.
    Use special insulating ink: Apply an insulating protective ink with a thickness greater than 30 micrometers (such as transparent green ink ED452SS) on the silver circuits as a physical barrier to prevent water vapor from invading.
    Introduce moisture absorption and superhydrophobic designs: For specific scenarios, a dedicated moisture-absorbing layer can be set between the signal lines and the ground lines to actively absorb water vapor; or an ultra-hydrophobic coating can be applied on the electrodes to prevent water from adhering and penetrating.

    III. Improving Circuit and Structural Design
    Increase safety distance: Try to widen the gap between the silver circuits (wires) as much as possible (for example, the gap between GND and TX0 should be at least 0.15mm). This will reduce the electric field strength and decrease the driving force for silver ions.
    Maintain low voltage operation: Within the design limits, keep the circuit in a low voltage (potential) state to reduce the rate of electrochemical migration.
    Add exhaust holes: Reasonably design exhaust holes around the membrane switch to prevent internal moisture from accumulating and accelerating migration.

    IV. Strictly Control Production and Drying Processes
    Standardize the drying procedure: Adopt a scientific stepwise drying method (such as first curing at a normal temperature for 2/3 of the time, leaving it at room temperature for 1-2 hours, and then conducting infrared drying). This ensures that the resin fully cross-links, avoiding insulation performance degradation due to insufficient curing or excessive solvents.
    Control the cleanliness of the workshop: When applying the insulating coating by screen printing, it is necessary to avoid the generation of dust and pinholes. Dust and debris falling between the wires can become channels for ion migration under specific conditions, causing electrical performance degradation.
    Thoroughly clean after laser engraving: If laser engraving is involved, after processing, it must undergo ultrasonic cleaning and be dried thoroughly (it is recommended to use pure water with resistivity ≤ 18.25), to prevent the residue of silver paste from causing short circuits.