How to optimize the thickening design of the contact area?
The thickening design of the contact area is a key means to enhance the lifespan and reliability of membrane switches. The core idea is to locally increase the thickness of the conductive layer in the contact area, while taking into account conductivity, wear resistance and process feasibility. Here is a systematic optimization plan:

Double-layer structure of silver paste and carbon paste (the most mainstream solution)
This is the most widely adopted contact thickening solution in the current industry, which takes into account both conductivity and wear resistance:
Bottom layer silver paste: Responsible for signal transmission, the dry film thickness is controlled at 7-12 μm to ensure a low contact resistance (< 3 Ω).
Top layer carbon paste: A conductive carbon paste is covered on the silver paste contact area through secondary printing, with a thickness controlled at 5-10 μm. After carbon paste curing, it has high hardness and excellent wear resistance, capable of withstanding more than 1 million mechanical friction, and providing self-lubrication effect.
Key process requirements: The silver paste layer must be fully cured before printing the carbon paste; otherwise, the silver powder particles will contaminate the carbon paste, resulting in an increase in sheet resistance.
Local secondary thickening
Selective thickening is carried out in the contact area instead of thickening the entire layer:
Window design of the screen: A special thickening screen is made, with windows only in the contact area, achieving precise local thickening.
Double printing stacking: The same contact area is printed with two layers of silver paste successively, and the total thickness of the dry film can reach 15-20 μm, significantly increasing the wear resistance margin.
Thickness control of photoresist: The thickness of the photoresist on the contact area screen is recommended to be 25-35 μm (higher than the 15-25 μm of the ordinary circuit layer), by increasing the thickness of the adhesive layer to increase the single ink deposition amount.
Edge transition treatment: A gradual transition design needs to be made between the thickened area and the normal thickness area to avoid stress concentration and delamination caused by thickness sudden change.
Gradient functional material contacts (high-end solution)
Suitable for high-reliability scenarios such as industrial control and medical equipment:
Underlying high-conductivity silver paste: Ensures signal transmission efficiency, with resistivity < 0.5 Ω·cm.
Surface noble metal protective layer: Covers a 0.5 - 1.27 μm layer of gold or palladium alloy, utilizing the chemical inertness of noble metals to inhibit oxidation and migration.
Performance data: A membrane switch with 0.5 μm gold-coated silver contacts, after 1 million rated load (12VDC, 100mA) pressing tests, the contact resistance increment is only 2 mΩ, much lower than the 15 mΩ increment of pure silver contacts.
Contact shape and area optimization
Thickening is not just a matter of "thickness"; the geometric design of the contacts is equally crucial:
Contact diameter design: It is recommended to have a contact diameter of 2 to 4 mm. If it is too small, the contact pressure will be too high, accelerating wear; if it is too large, the force required for operation will increase and it will affect the layout density.
Ring-shaped contact structure: Design the contacts as a ring (instead of a solid circle), increasing the effective contact perimeter with the same amount of silver paste, and distributing wear.
Dimple design: Press a small raised dot (height 0.05 to 0.1 mm) at the center of the contact, concentrating the contact in the raised dot area. The initial contact pressure is sufficient to pierce the oxide film, and after the raised dot wears out, there is still enough silver paste remaining.
Collaborative optimization of process parameters
For the thickening design, the printing process parameters need to be adjusted accordingly:
| Parameter | Ordinary circuit layer | Contact thickening layer | Adjustment purpose |
| Mesh count | 200-250 mesh | 150-200 mesh | Reduce mesh count to increase ink deposition amount |
| Photographic film thickness | 15 - 25 μm | 25 - 35 μm | Increases ink storage capacity |
| Scraping knife hardness | 70-75 Shore A scale | 65-70 Shore A scale | Soft scraping knife increases ink deposition |
| Scraping tool angle | 60° - 75° | 45° - 60° | Small angle increases film thickness |
| Printing speed | 40 - 150 mm/s | 30 - 80 mm/s | Gradually increase deposition amount |
| Number of printings | 1 time | 2-3 times | reaching the target thickness through multiple layers |
Quality control key points
Thickness uniformity: The thickness deviation of the thickened area should be controlled within ±15%, and the thickness at the center and edge of the contact point should be measured at three points each using a film thickness gauge and the average value should be taken.
Resistance verification: After thickening, the resistance of the contact area should be <30 mΩ/□ (pure silver paste) or <100 mΩ/□ (silver + carbon double layer).
Adhesion test: The thickened area must pass the 3M 800 tape test without peeling to be qualified.
Sufficient curing: The solvent evaporation path of the thickened layer is longer. The curing temperature is recommended to be 5-10°C higher than that of the ordinary layer or the curing time is extended by 30-60 seconds to ensure complete curing of the underlying layer.
Summary: The core of the thickened contact design is "silver base carbon surface double-layer structure + local secondary printing + geometric shape optimization". For general consumer electronics, a single printing of silver paste + carbon paste coverage can meet the requirements; for industrial-grade products, it is recommended to use a secondary printing of silver paste to thicken to 15-20 μm before covering with carbon paste, combined with bump design, which can increase the contact life from 500,000 times to over 5 million times. When implementing the thickening design, it is essential to pay attention to the sufficiency of curing and interlayer adhesion to avoid the detachment of the thickened layer due to improper processing.