    What are the requirements for the printing of insulating ink on membrane switches?

    2026-06-24

    The printing of insulating ink on membrane switches is a crucial process for ensuring the safety and reliability of the circuit. Its core function is to isolate and protect the silver paste lines, and to prevent short circuits and silver paste migration. The main technical requirements for insulating ink printing are as follows: 

    productive process (4).jpg

    Selection of insulating ink types

    Insulating ink is divided into two types: solvent-based and UV-curable. 
    Solvent-based: Uses vinyl resin or polyester resin as the base material and is cured through heating and drying. The process is mature and the cost is relatively low.
    UV-curable type: Cured by ultraviolet light irradiation. The film thickness is more uniform and the insulation performance is better. When the film thickness is 20 μm, the insulation resistance can reach 3×10¹¹ Ω, and when the film thickness is 35 μm (after two printing) it can reach 3×10¹² Ω. 
    It is recommended to prefer UV-curable type, as it offers more stable insulation performance and a faster curing speed, making it suitable for mass production.

    Coverage requirements (the most critical) 
    The coverage range of insulating ink follows two fundamental rules: 
    Full coverage is mandatory: The insulating ink must completely cover all the silver paste circuits, and there must be no exposed silver paste areas; otherwise, it will cause short circuits between the circuits or silver paste migration.
    No coverage of contacts: No insulating ink shall be attached to the contact points (silver paste contact areas) of all membrane switches; otherwise, the buttons will not conduct electricity.

    Film thickness and insulation performance

    Film thickness  Insulation resistance  Explanation
    20 μm (single printing)  ≥ 3 × 10¹¹ Ω Minimum requirement for routine applications
    35 μm (two printings) ≥ 3 × 10¹² Ω   Recommended for high-reliability applications
    Above 50 μm  ≥ 10¹³ Ω Special high-voltage scenarios

    Industry standard requirements: Insulation resistance ≥ 100 MΩ (100V/DC), substrate withstand voltage ≥ 2kV (DC).
    Practical application suggestions: For regular products, the thickness of the insulation ink should be controlled within 20-35 μm. For high-reliability products (such as medical and military applications), it is recommended to achieve a thickness of more than 35 μm after two printing processes. 
    Printing quality requirements

    The appearance and performance of the ink printed with insulating oil must meet the following standards: 
    Smooth surface: There must be no bubbles, pinholes or other defects, otherwise the insulation effect will be seriously affected.
    No ink spread: The ink edges must not spread, and the handwriting must be complete.
    Printing accuracy: Dimension deviation ≤ ±0.10mm, color registration deviation ≤ ±0.11mm/100mm.
    Transparency rate: For UV-cured transparent insulating ink, the transparency rate ≥ 90% (especially important when backlighting is required).
    Breakdown voltage: ≥ 10kV/mm.

    Printing process parameters 
    Screen mesh count: The insulating layer uses 110-156 mesh (43-61 threads/cm) mesh fabric, providing a relatively thick ink deposition amount (0.001-0.002 inches).
    Scraping knife hardness: 70-80 Shore A polyurethane scraping knife, with a blade angle of 60°.
    Printing pressure: 2-5 kgf. Excessive pressure causes ink diffusion, while too little pressure results in incomplete coverage.
    Cutting speed: 30-60 mm/s.
    Environmental control: Temperature 23 ± 2℃, humidity 50 ± 5%, low humidity is prone to generating static electricity and causing ink flying.

    Common Questions and Solutions 
    Bubbles/holes: The main cause is either excessively high ink viscosity or too fast printing speed. Solution: Reduce the ink viscosity appropriately, slow down the cutting speed, and let the printed product stand and level for 5 to 10 minutes before curing.
    Incomplete coverage: The silver paste lines have exposed edges. Solution: The coverage area of the insulating ink should be 0.3 to 0.5 mm wider than the edge of the silver paste lines as a safety margin.
    Incorrect coverage of contacts: Insulating ink has invaded the contact area. Solution: During plate making, reserve a 0.5 to 1.0 mm isolation margin in the contact area to ensure alignment accuracy.
    Incomplete curing: Insufficient UV energy or too fast curing speed. Solution: Ensure that the UV energy reaches 800 to 1200 mJ/cm², and the curing speed is controlled at 10 to 15 m/min.

    💡 Summary: The core requirements for insulating ink printing are complete coverage of silver paste lines, zero coverage of contact areas, film thickness of 20-35 μm, and no bubbles or pinholes. During the design process, the coverage area of the insulating ink should be expanded by 0.3-0.5 mm beyond the silver paste lines as a safety margin, and a 0.5-1.0 mm isolation margin should be reserved for the contact areas. After printing, it is necessary to test whether the insulation resistance meets the standard (≥100 MΩ) to ensure the safety and reliability of the circuit.