What effect does the curing temperature have on conductivity?
In the production of membrane switches, the curing temperature has a decisive influence on the electrical conductivity of conductive pastes (such as silver paste, carbon paste). The electrical conductivity of the conductive coating mainly depends on the close contact between the conductive filler (such as silver powder, carbon powder) particles to form a conductive path, and the curing temperature directly determines the shrinkage rate of the resin, the degree of solvent evaporation, and the sintering state of the particles.
Specifically, the influence of curing temperature on conductivity is mainly reflected in the following aspects:

1. Insufficient temperature: The conductive network fails to form, resulting in high resistance.
When the curing temperature is insufficient, the resin cannot fully cross-link and the solvent cannot completely evaporate.
Poor particle contact: If the resin is not fully cured, the conductive powder will be encapsulated in loose resin, and particles cannot form a tight contact (i.e., lacking "neck contraction" connection), leading to extremely high contact resistance.
Unstable performance: In the carbon paste process, if the curing temperature is below 130℃, the binder is not fully cured, which will result in high resistance and extremely poor stability.
2. Appropriate Temperature: Resin Shrinkage and Particle Sintering, Conductivity Achieves Optimal Level
Within the recommended curing temperature range, the conductivity will significantly improve as the temperature rises and then stabilize after reaching the optimal value.
Promoting Volume Shrinkage: Appropriate high temperatures are conducive to the shrinkage movement of the resin. The volume shrinkage of the resin during the curing process generates strong compressive stress, prompting the silver powder or carbon powder particles to closely contact each other, thereby significantly reducing the volume resistivity.
Promoting Sintering and Organic Matter Decomposition: For materials such as nano-silver powder, high temperatures can trigger particle sintering, significantly accelerating the growth rate of the sintering neck. At the same time, high temperatures are beneficial for the evaporation and decomposition of the organic layer on the surface of the silver powder, further reducing the contact resistance between the powder particles.
Optimal Process Window: For example, when carbon oil is cured at 150℃ for 30 minutes, the resistance is the lowest and the stability is the best; for nano-silver ink, when coupled with photothermal curing (substrate at 160℃), the resistivity can be reduced to an extremely low level (3.75 μΩ·cm).
3. Excessive temperature: Material oxidation and structural damage, deterioration of conductivity
The curing temperature is not necessarily the higher the better. Once it exceeds the material's tolerance limit, the conductivity will not increase but decrease instead.
Oxidation of conductive particles: Excessive temperature (such as carbon paste exceeding 170℃) will cause carbon powder or silver powder to undergo oxidation reactions, generating non-conductive oxide layers, resulting in a 5%-10% or even greater increase in resistance.
Resin thermal decomposition: Excessively high temperature may cause the matrix resin to undergo thermal degradation, destroying the dense structure of the coating and leading to the breakdown of the conductive pathways.
4. Synergistic effect of curing time and environment
Time synergy: The curing temperature and curing time are usually positively correlated. Within a certain range, the higher the curing temperature and the longer the curing time, the better the conductivity, until a stable value is reached.
Environmental factors: If the cured coating is in a humid environment (such as 85% relative humidity), water vapor will penetrate and obstruct the pathways between the conductive particles, resulting in a significant increase in resistance (possibly rising by 20%). Therefore, the moisture-proof protection after curing is crucial for maintaining conductivity.
Summary:
In the production of membrane switches, to achieve the best conductivity performance, the curing temperature must be controlled within an appropriate range (usually following the stepwise heating method). This not only ensures that the resin fully contracts and promotes the close contact and sintering of the conductive particles, but also effectively avoids the problems of particle oxidation and resin degradation caused by high temperatures.