Welcome to LuphiTouch®!
Today is 2026.11.05 , Thursday
Leave Your Message
News Categories
    Featured News

    What factors can affect the conductive silver paste of the membrane switch?

    2026-06-15

    The performance of the conductive silver paste in membrane switches is extremely sensitive. Its final performance (such as conductivity, adhesion, and long-term reliability) is influenced by multiple dimensions including material formulation, printing process, and environmental factors. Specifically, it is mainly affected by the following key factors:

    productive process (14).jpg

    1. Material formulation and component characteristics
    Silver content: The silver content of silver paste is usually above 60% to 90%. The higher the silver content, the closer the contact between the conductive particles, and generally better conductivity and lower volume resistivity can be achieved.
    Resin and solvent system: The types of binder resin and organic solvents determine the adhesion of the silver paste, the flexibility of the cured film, and the thixotropy. For example, the application of mixed resins can make up for the deficiencies in adhesion or flexibility of a single resin; while mixed solvents can optimize the solubility and the volatility gradient during the curing process, thereby improving the quality of the cured film.
    Environmental compliance (halogen control): Traditional formulations may contain excessive halogens (such as bromine and chlorine), which not only do not meet modern environmental requirements but may also affect the stability of the material. Strictly controlling the halogen content in the resin can ensure the quality and safety of the silver paste from the source.
    Particle size distribution: Finer silver powder particles can achieve higher resolution printing, but if not coated properly, it will increase the oxidation risk.

    2. Printing Process Parameters
    Viscosity Control: Viscosity directly affects the printing quality and film thickness. Silver paste with low viscosity is more suitable for screen printing, while high viscosity is better for dispensing. The accuracy of rheological control determines whether the lines are uniform, whether there are burrs or gaps.
    Curing Temperature and Time: This is the core aspect determining the final performance of the silver paste. Appropriate curing temperature can promote the full cross-linking of the resin and allow the silver powder to closely contact each other, thereby reducing resistance and enhancing adhesion; if the temperature is too low, the conductive network will not form, and if it is too high, the material may undergo thermal degradation or be damaged by thermal stress.
    Environmental Humidity: Silver paste is extremely sensitive to humidity. Many silver pastes will absorb moisture and degrade in a humid environment, resulting in a significant decline in performance. Therefore, the humidity of the production and storage environment must be strictly controlled.

    3. Environmental and Mechanical Stress Factors
    Temperature and Humidity Aging: Membrane switches will encounter challenges related to working temperature and humidity in practical applications. In high-temperature and high-humidity environments (such as 55℃ and 90% humidity), if the silver paste has poor resistance to migration, it is highly likely to cause silver ion migration and result in short circuits; at the same time, the infiltration of water vapor will also impede the pathways between conductive particles, increasing the resistance.
    Mechanical Fatigue and Flexibility: Membrane switches need to withstand frequent pressing operations (such as more than 1 million cycles of service life). This requires the conductive silver paste to have excellent flexibility and fatigue resistance to withstand bending tests without breaking or experiencing a significant increase in resistance.

    Base material compatibility: The silver paste must have good compatibility and adhesion with the flexible base materials commonly used in membrane switches (such as PET polyester film, polycarbonate, etc.). Otherwise, it is prone to delamination and detachment under force or environmental changes.