    What is the light transmittance of the membrane button panel typically?

    2026-05-18

    The light transmittance of the membrane button panel is not a fixed value. It depends on the material type, processing method, and functional requirements.

    machinery equipment (2).jpg
    Generally speaking, the light transmittance of ordinary transparent films is between 85% and 92%, while specially treated high-end optical films can reach over 95%.
    To enable you to make a more accurate assessment, I have compiled the light transmittance data under different circumstances as follows:

    1. Light transmittance benchmarks for different materials
    The commonly used base materials for membrane button panel mainly include PET, PC and PVC. Their light transmittance properties vary:
    PET (Polyester):
    Light transmittance: Usually between 88% and 92%.
    Characteristics: This is the most commonly used film material, with balanced optical performance. High-end optical-grade PET can even reach 94%.
    PC (Polycarbonate):
    Light transmittance: Usually between 85% and 90%.
    Characteristics: Although the light transmittance is slightly lower than PET, it has extremely strong impact resistance. The PC material itself tends to yellow, so high-end PC panels usually add a hard coating to maintain the light transmittance.
    PVC (Polyvinyl Chloride):
    Light transmittance: Generally between 80% and 90%.
    Characteristics: Mostly used for low-end or simple decorative panels, with relatively poor optical performance.

    productive process (14).jpg

    2. The influence of surface treatment on light transmittance
    Membrane button panel rarely use "bare film" directly. The surface treatment process significantly alters the light transmittance:
    Matte treatment (Sanded/Frosted):
    Light transmittance: 80% - 88%.
    Impact: The matte surface will cause light scattering (increased glossiness), which makes the picture appear soft and anti-glare, but it will sacrifice a portion of the light transmittance, making the displayed content appear slightly "blurry".
    Glossy/Hardening treatment (Glossy/HC):
    Light transmittance: 90% - 92%.
    Impact: The surface is smooth, and the direct light transmission rate is high, the picture is clear and bright, but it is prone to reflection.
    Anti-reflective coating (AR):
    Light transmittance: > 95% - 98%.
    Impact: This is a high-end process (such as mobile phone screens, high-end vehicle screens), through nano-coating to reduce light reflection, greatly improving light transmittance, and can be clearly seen even in strong light.

    3. Special Cases of Functional Films
    If your panel has special functions, the transmittance will vary significantly:
    Transparent Conductive Film (ITO):
    Used for touch screens or for heating and de-icing, the transmittance is usually required to be > 80%. High-end ITO films can have a transmittance of 90% to 98% at a wavelength of 550nm.
    LED Crystal Film Screen (Display Type):
    This new type of film screen can have a transmittance of over 90% when it is off, almost like transparent glass.

    Summary and Recommendations
    General standard: If you are making ordinary industrial or household panels, a transmittance of ≥ 85% is considered a qualified and common level.
    High-end requirements: If you need high-definition display (such as medical equipment, high-end vehicle screens), it is recommended to choose optical-grade PET or PC, and the transmittance should be ≥ 90%. It is best to add an AR anti-reflective coating.
    Note on haze: Do not only focus on the transmittance, but also pay attention to the haze (Haze). If the transmittance is high but the haze is also high (> 1%), the picture will appear white and unclear.


    One-sentence advice: On the custom drawing, it is recommended to mark "Transmittance ≥ 88% (or according to your requirements)" and clearly indicate whether "low haze" or "anti-glare" treatment is needed, to avoid the resulting panels looking grayish.