    What is the specific process for the high-temperature test of the membrane switch panels?

    2026-05-15

    The high-temperature resistance test of the membrane switch panels is not a single action but a rigorous "aging - cooling - inspection" process. This process aims to simulate whether the panel will experience failure phenomena such as blistering, delamination, deformation or color change under long-term high temperatures or extreme temperature differences.

    According to industry standards (such as GB/T, ASTM, IEC) and laboratory routine

    operations, the specific test process is as follows:

    machinery equipment (13).jpg
     Stage 1: Preparations before the test

    Before placing the panel in the oven, the following preparations must be completed to ensure the accuracy of the test data:

    1. Sample Preparation:

    Randomly select at least 3-5 finished panels (or standard splines) from the same batch.

    For finished product testing, it is recommended to include the complete structure (panel + adhesive + base plate).


    2. Initial Inspection (Establishing a Benchmark):

    Appearance Inspection: Record the initial color, gloss, and confirm there are no bubbles or scratches.

    Dimension Measurement: Measure the length, width, and thickness of key areas and record the initial data.

    Function Testing: If the panel has a circuit, it is necessary to test the initial conduction resistance and button feel (force).


    3. Equipment Setup:

    Use a forced convection drying oven (oven).

    Set the temperature: Based on the material grade, set it (PET usually at 80°C - 100°C, PC at 100°C - 120°C, PI at 150°C - 200°C).

    Set the time: Usually 168 hours (7 days), 500 hours, or 1000 hours.

    Phase 2: High-temperature exposure (aging process)

    This is the core part of the test, simulating a long-term exposure to heat:

    1. Inserting the samples:

    Preheat the oven to the set temperature and keep it stable for at least 30 minutes.

    Place the samples on a metal grid inside the oven (do not touch the box walls directly).

    Key point: Samples should be kept at a certain distance from each other (usually ≥ 10mm), and they should not be stacked to ensure free circulation of hot air.

    2. Maintaining constant temperature:

    Close the oven door and start timing.

    The oven must maintain a temperature fluctuation within ±1°C to ensure uniform heating.

    During this period, unless otherwise specified by the standard (such as air exchange aging), generally it is not allowed to open the oven door to avoid sudden temperature drops that may affect the test results.

    Phase 3: Cooling and Recovery

    After the testing period is over, performance testing cannot be conducted immediately. The material must be allowed to "cool down":

    1. Remove the sample: Take the sample out of the oven.

    2. Natural cooling: Place the sample in a desiccator or at room temperature for natural cooling.

    3. State adjustment: Usually, it is required to leave the sample at room temperature (23 ± 2°C) for 24 hours.

    Objective: To eliminate the temporary stress caused by thermal expansion and contraction, allowing the material's performance to return to a stable state, so that subsequent measurements can be carried out.

    Phase 4: Performance Evaluation (Failure Determination)

    The cooled samples will undergo a comprehensive "check-up", mainly examining the following four aspects:

    Detection Dimension Specific Item Determination Criteria (Reference)
    Appearance Visual Inspection    No blistering, no delamination, no cracks, no deformation.  The color change on the surface (ΔE) is usually required to be < 2.0.
    Size Length/Width/Thickness Dimension change rate is usually required to be ≤ 1% (more strict requirements for precision components).
    Mechanical Adhesion/Hardness Perform a hundred-grid test using 3M 610 adhesive tape, and the ink should not fall off; the pencil hardness should not show a significant decrease.
    Function Conduction/Feel Circuit resistance change rate < 5%; the feel of the buttons should not show significant softening or collapse.

    Special process: High and Low Temperature Shock Test

    If your panel is used in vehicles or outdoors, in addition to the above constant temperature aging, a cold and hot shock process is usually required as well:

    1. Cycling settings: For example, -40°C (2 hours) ⇋ 90°C (2 hours).
    2. Transition time: The time required for transitioning from high temperature to low temperature (or vice versa) is usually within 5 minutes.
    3. Number of cycles: Usually, 10, 50, or 100 cycles are performed.
    4. Purpose: Mainly to detect delamination or cracking of different material layers (such as ink, film, glue) caused by the different expansion coefficients.

    productive process (8).jpg

    Summary and suggestions: For routine quality control, conducting a 168-hour (7-day) 85°C constant temperature aging test is the most universal and effective solution. If your panel involves precision displays (such as LCD windows), after the test, it is essential to carefully inspect the edges of the window for any overflow or contraction phenomena.